Wrought alloy (bar, rod, sheet, forging) · Japan · JIS H 4000 / H 4040
A1050 Commercially pure 1050A
A1050 (Commercially pure 1050A) is a wrought commercially pure 1050a alloy to JIS H 4000 / H 4040, in the pure aluminum (1xxx) group. Nominal composition: Al >= 99.5. Typical uses: busbar, sheet, chemical plant. Equivalents: AA 1050A (A91050) (USA), EN AW-1050A (Al99,5) (Europe), Al99.5 (3.0255) (Germany), 1B (UK).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/a1050
A1050 Commercially pure 1050A
JIS H 4000 / H 4040
Chemical composition
A1050 — nominal composition
Weight %, to JIS H 4000 / H 4040. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Al | ≥ 99.5 |
Mechanical & physical properties
A1050 — properties
Values shown are for 1050A, the same alloy in another standard. Limits for A1050 may differ slightly — the standard on your drawing governs.
| Tensile strength, typical | 115 MPa |
| Yield / 0.2 % proof stress, typical | 105 MPa |
| Elongation, typical | 7 % |
| Brinell hardness, typical | 34 HB |
| Density at 20 °C | 2.705 g/cm³ |
| Melting range (solidus–liquidus) | 645–658 °C |
| Electrical conductivity at 20 °C | 61 % IACS |
| Thermal conductivity at 20 °C | 229 W/m·K |
Source: H14, Aluminum Association typical (typical values).
International equivalents
A1050 cross-reference
| System | Designation |
|---|---|
| Japan (this grade) | A1050 · Commercially pure 1050A |
| USA · UNS / ASTM | AA 1050A (A91050) |
| Europe · EN | EN AW-1050A (Al99,5) |
| Germany · DIN | Al99.5 (3.0255) |
| UK · BS | 1B |
| China · GB | — |
⚠️ Relationship: Family match. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ Busbar
- ▸ Sheet
- ▸ Chemical plant
Product forms: Bar, extrusion, plate, sheet
A1050 parts
A1050 is a wrought grade (bar, rod, forging): we supply parts CNC machined from bar or forged — it is not used for castings. For a cast part, choose a cast grade.
Same alloy in other standards
Grades from the same cross-reference group.
More pure aluminum (1xxx)
Specification
How to specify A1050 on a drawing or order
- ▸ Grade and standard: JIS H 4000 / H 4040 – A1050 / Commercially pure 1050A.
- ▸ Temper and size: state the temper (for example R360 / H080) when strength or hardness matters.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204
A1050 — questions buyers ask
What is A1050?+
A1050 (Commercially pure 1050A) is a wrought commercially pure 1050a alloy to JIS H 4000 / H 4040, in the pure aluminum (1xxx) group. Nominal composition: Al >= 99.5. Typical uses: busbar, sheet, chemical plant. Equivalents: AA 1050A (A91050) (USA), EN AW-1050A (Al99,5) (Europe), Al99.5 (3.0255) (Germany), 1B (UK).
What are the equivalents of A1050?+
USA: AA 1050A (A91050); Europe: EN AW-1050A (Al99,5); Germany: Al99.5 (3.0255); UK: 1B. Relationship: Family match. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of A1050?+
Tensile strength, typical: 115 MPa; Yield / 0.2 % proof stress, typical: 105 MPa; Elongation, typical: 7 %; Brinell hardness, typical: 34 HB. Source: H14, Aluminum Association typical (typical values).
Does Conex supply parts in A1050?+
A1050 is a wrought grade (bar, rod, sheet or forging stock). We machine and supply finished parts in it to your drawing, and can recommend the matching cast grade if you need a casting instead.
How do I specify A1050 on a drawing?+
Write the standard and the grade together, for example "JIS H 4000 / H 4040 – A1050 (Commercially pure 1050A)", and the temper. Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: JIS H 4000 / H 4040 — Current.
- ▸ Properties: H14, Aluminum Association typical (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order A1050
Indicative $5/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.