Casting alloy · Japan · JIS H 5120

CAC701 AlBC1

CAC701 (AlBC1) is a casting aluminum bronze / nickel aluminum bronze alloy to JIS H 5120 (castings) / JIS H 5121 (continuous cast, suffix 'C'), in the aluminum & nickel-aluminum bronze group. Nominal composition: Cu 85–90, Al 8–10, Fe 1–3, Ni ≤ 1, Mn ≤ 1. Typical uses: propellers, seawater pumps & valves, gears, chemical-plant parts. Equivalents: C95200 (USA), CC331G CuAl10Fe2-C (Europe), G-CuAl10Fe (Germany), AB1 (UK).

Casting alloyJapanAluminum bronze / nickel aluminum bronzeCurrent standardData: US equivalent C95200

Chemical composition

CAC701 — nominal composition

Weight %, to JIS H 5120 (castings) / JIS H 5121 (continuous cast, suffix 'C'). Single values are maximums unless marked. The full limits (impurities) are in the standard.

ElementWeight %
Cu85–90
Al8–10
Fe1–3
Ni≤ 1
Mn≤ 1

Mechanical & physical properties

CAC701 — properties

Values shown are for the nearest US grade C95200. JIS limits for CAC701 may differ slightly — the standard on your drawing governs.

Tensile strength, min.469 MPa
Yield strength (0.5 % ext.), min.179 MPa
Elongation in 50 mm, min.20 %
Brinell hardness (500 kg), typical125 HB
Density at 20 °C7.64 g/cm³
Melting range (solidus–liquidus)1042–1045 °C
Electrical conductivity at 20 °C11 % IACS
Thermal conductivity at 20 °C50.4 W/m·K
Thermal expansion (20–200 °C)15.5 ×10⁻⁶/K
Modulus of elasticity103 GPa
Machinability rating20 (free-cutting brass C36000 = 100)

Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).

International equivalents

CAC701 cross-reference

SystemDesignation
Japan (this grade)CAC701 · AlBC1
USA · UNS / ASTMC95200 / C95400 (nearest)
Europe · ENCC331G CuAl10Fe2-C
Germany · DING-CuAl10Fe
UK · BSAB1
China · GBZCuAl10Fe3

⚠️ Relationship: Nearest. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.

Typical applications

  • ▸ Propellers
  • ▸ Seawater pumps & valves
  • ▸ Gears
  • ▸ Chemical-plant parts

Casting methods: Sand, mold, centrifugal, continuous

How we cast CAC701

Every casting machined and inspected in-house.

Same alloy in other standards

Grades from the same cross-reference group.

In-depth guide

Aluminum Bronze AB1

Processes, parts, industries and prices for this alloy at Conex.

Read the Aluminum Bronze AB1 guide →

Specification

How to specify CAC701 on a drawing or order

  • ▸ Grade and standard: JIS H 5120 – CAC701 / AlBC1.
  • ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
  • ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
  • ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.

Buyer guides: EN 10204 · ISO 8062-3

CAC701 — questions buyers ask

What is CAC701?+

CAC701 (AlBC1) is a casting aluminum bronze / nickel aluminum bronze alloy to JIS H 5120 (castings) / JIS H 5121 (continuous cast, suffix 'C'), in the aluminum & nickel-aluminum bronze group. Nominal composition: Cu 85–90, Al 8–10, Fe 1–3, Ni ≤ 1, Mn ≤ 1. Typical uses: propellers, seawater pumps & valves, gears, chemical-plant parts. Equivalents: C95200 (USA), CC331G CuAl10Fe2-C (Europe), G-CuAl10Fe (Germany), AB1 (UK).

What are the equivalents of CAC701?+

USA: C95200 / C95400 (nearest); Europe: CC331G CuAl10Fe2-C; Germany: G-CuAl10Fe; UK: AB1; China: ZCuAl10Fe3. Relationship: Nearest. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.

What is the tensile strength of CAC701?+

Tensile strength, min.: 469 MPa; Yield strength (0.5 % ext.), min.: 179 MPa; Elongation in 50 mm, min.: 20 %; Brinell hardness (500 kg), typical: 125 HB. Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).

Can Conex cast CAC701?+

Yes. We cast CAC701 by sand casting, centrifugal casting, continuous casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.

How do I specify CAC701 on a drawing?+

Write the standard and the grade together, for example "JIS H 5120 – CAC701 (AlBC1)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.

Sources & references

  • ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
  • ▸ Controlling standard: JIS H 5120 (castings) / JIS H 5121 (continuous cast, suffix 'C').
  • ▸ Properties: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
  • ▸ Always verify against the current edition of the standard for contract or safety-critical parts.

Order CAC701

Indicative $14/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation

Send your drawing, get a quotation.

DWG, PDF, STEP or a sample photo — with quantity and destination port.

All productsGet quote
☎Call✉Email⬇CatalogueGet Quote
Conex

Conex Export Desk

Talk to our export team

Working on a new casting? Tell us the part and we'll connect you with the right engineer today.