ConexCONEXCASTING FOUNDRY

Casting alloy · Europe · EN 1982:2017

CC491K CuSn5Zn5Pb5-C

CC491K (CuSn5Zn5Pb5-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the gunmetal & red brass group. Nominal composition: Sn 4–6, Zn 4–6, Pb 4–6, Cu rem (85-5-5-5). Typical uses: valves & pumps up to ~225 °C, general bearings. Equivalents: C83600 (USA), G-CuSn5ZnPb (Rg5) (Germany), LG2 (UK), CAC406 (Japan).

Casting alloyEuropeLeaded / bearing bronzeCurrent standardData: US equivalent C83600

Chemical composition

CC491K — nominal composition

Weight %, to EN 1982:2017 (ingots CB…-B / castings CC…-C). Single values are maximums unless marked. The full limits (impurities) are in the standard.

ElementWeight %
Sn4–6
Zn4–6
Pb4–6
Curem (85-5-5-5)

Mechanical & physical properties

CC491K — properties

Values shown are for the nearest US grade C83600. EN limits for CC491K may differ slightly — the standard on your drawing governs.

Tensile strength, min.248 MPa
Yield strength (0.5 % ext.), min.131 MPa
Elongation in 50 mm, min.15 %
Brinell hardness (500 kg), typical60 HB
Density at 20 °C8.83 g/cm³
Melting range (solidus–liquidus)854–1010 °C
Electrical conductivity at 20 °C15 % IACS
Thermal conductivity at 20 °C72 W/m·K
Thermal expansion (20–200 °C)17.3 ×10⁻⁶/K
Modulus of elasticity93 GPa
Machinability rating84 (free-cutting brass C36000 = 100)

Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).

International equivalents

CC491K cross-reference

SystemDesignation
Europe (this grade)CC491K · CuSn5Zn5Pb5-C
USA · UNS / ASTMC83600
Germany · DING-CuSn5ZnPb (Rg5)
UK · BSLG2
Japan · JISCAC406
China · GBZCuSn5Pb5Zn5

⚠️ Relationship: Published comparison. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.

Typical applications

  • ▸ Valves & pumps up to ~225 °C
  • ▸ General bearings

Casting methods: GS, GM, GZ, GC (sand, permanent mold, centrifugal, continuous)

How we cast CC491K

Every casting machined and inspected in-house.

Same alloy in other standards

Grades from the same cross-reference group.

In-depth guide

Gunmetal LG2 / CC491K

Processes, parts, industries and prices for this alloy at Conex.

Read the Gunmetal LG2 guide →

Specification

How to specify CC491K on a drawing or order

  • ▸ Grade and standard: EN 1982:2017 – CC491K / CuSn5Zn5Pb5-C.
  • ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
  • ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
  • ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.

Buyer guides: EN 1982 · EN 10204 · ISO 8062-3

CC491K — questions buyers ask

What is CC491K?+

CC491K (CuSn5Zn5Pb5-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the gunmetal & red brass group. Nominal composition: Sn 4–6, Zn 4–6, Pb 4–6, Cu rem (85-5-5-5). Typical uses: valves & pumps up to ~225 °C, general bearings. Equivalents: C83600 (USA), G-CuSn5ZnPb (Rg5) (Germany), LG2 (UK), CAC406 (Japan).

What are the equivalents of CC491K?+

USA: C83600; Germany: G-CuSn5ZnPb (Rg5); UK: LG2; Japan: CAC406; China: ZCuSn5Pb5Zn5. Relationship: Published comparison. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.

What is the tensile strength of CC491K?+

Tensile strength, min.: 248 MPa; Yield strength (0.5 % ext.), min.: 131 MPa; Elongation in 50 mm, min.: 15 %; Brinell hardness (500 kg), typical: 60 HB. Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).

Can Conex cast CC491K?+

Yes. We cast CC491K by sand casting, gravity die casting, centrifugal casting, continuous casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.

How do I specify CC491K on a drawing?+

Write the standard and the grade together, for example "EN 1982:2017 – CC491K (CuSn5Zn5Pb5-C)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.

Sources & references

  • ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
  • ▸ Controlling standard: EN 1982:2017 (ingots CB…-B / castings CC…-C).
  • ▸ Properties: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
  • ▸ Always verify against the current edition of the standard for contract or safety-critical parts.

Order CC491K

Indicative $13/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation

Send your drawing, get a quotation.

DWG, PDF, STEP or a sample photo — with quantity and destination port.

All productsGet quote
☎Call✉Email⬇CatalogueGet Quote
Conex

Conex Export Desk

Talk to our export team

Working on a new casting? Tell us the part and we'll connect you with the right engineer today.