Wrought alloy (bar, rod, sheet, forging) · Germany · DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672
2.0331 CuZn36Pb1.5
2.0331 (CuZn36Pb1.5) is a wrought leaded brass (machining) alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the free-cutting & forging brass group. Nominal composition: Cu 62-64, Pb 0.8-1.6, Zn rem. Typical uses: engraving, cold-headed and machined parts. Equivalents: C34000 (USA), CW600N CuZn35Pb1 (Europe), CZ118 (UK), C3501 (Japan).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/din-2-0331
2.0331 CuZn36Pb1.5
DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN
Chemical composition
2.0331 — nominal composition
Weight %, to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Cu | 62-64 |
| Pb | 0.8-1.6 |
| Zn | rem |
Mechanical & physical properties
2.0331 — properties
Values shown are for CW601N, the same alloy in another standard. Limits for 2.0331 may differ slightly — the standard on your drawing governs.
| Tensile strength, typical | 400 MPa |
| Yield / 0.2 % proof stress, typical | 280 MPa |
| Elongation, typical | 20 % |
| Brinell hardness, typical | 110 HB |
| Density at 20 °C | 8.47 g/cm³ |
| Melting range (solidus–liquidus) | 885–900 °C |
| Electrical conductivity at 20 °C | 26 % IACS |
| Thermal conductivity at 20 °C | 115 W/m·K |
| Machinability rating | 90 (free-cutting brass = 100) |
Source: rod, half hard, typical (typical values).
International equivalents
2.0331 cross-reference
| System | Designation |
|---|---|
| Germany (this grade) | 2.0331 · CuZn36Pb1.5 |
| USA · UNS / ASTM | C34000 |
| Europe · EN | CW600N CuZn35Pb1 |
| UK · BS | CZ118 |
| Japan · JIS | C3501 |
| China · GB | — |
⚠️ Relationship: Nearest. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs. This cross-reference should be verified against the controlling standard before certification.
Typical applications
- ▸ Engraving
- ▸ Cold-headed and machined parts
Product forms: Rod, bar, wire, sheet, strip, tube
2.0331 parts
2.0331 is a wrought grade (bar, rod, forging): we supply parts CNC machined from bar or forged — it is not used for castings. For a cast part, choose a cast grade.
More free-cutting & forging brass
Specification
How to specify 2.0331 on a drawing or order
- ▸ Grade and standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0331 / CuZn36Pb1.5.
- ▸ Temper and size: state the temper (for example R360 / H080) when strength or hardness matters.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204
2.0331 — questions buyers ask
What is 2.0331?+
2.0331 (CuZn36Pb1.5) is a wrought leaded brass (machining) alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the free-cutting & forging brass group. Nominal composition: Cu 62-64, Pb 0.8-1.6, Zn rem. Typical uses: engraving, cold-headed and machined parts. Equivalents: C34000 (USA), CW600N CuZn35Pb1 (Europe), CZ118 (UK), C3501 (Japan).
What are the equivalents of 2.0331?+
USA: C34000; Europe: CW600N CuZn35Pb1; UK: CZ118; Japan: C3501. Relationship: Nearest. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of 2.0331?+
Tensile strength, typical: 400 MPa; Yield / 0.2 % proof stress, typical: 280 MPa; Elongation, typical: 20 %; Brinell hardness, typical: 110 HB. Source: rod, half hard, typical (typical values).
Does Conex supply parts in 2.0331?+
2.0331 is a wrought grade (bar, rod, sheet or forging stock). We machine and supply finished parts in it to your drawing, and can recommend the matching cast grade if you need a casting instead.
How do I specify 2.0331 on a drawing?+
Write the standard and the grade together, for example "DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0331 (CuZn36Pb1.5)", and the temper. Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN — Legacy DIN designation (W.Nr still widely quoted).
- ▸ Properties: rod, half hard, typical (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order 2.0331
Indicative $9/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.