Wrought alloy (bar, rod, sheet, forging) · Europe · EN 573-3 / EN 485 / EN 755
EN AW-6082 EN AW-AlSi1MgMn
EN AW-6082 (EN AW-AlSi1MgMn) is a wrought al-si-mg-mn 6082 alloy to EN 573-3 / EN 485 / EN 755, in the al-mg-si (6xxx) - structural & machining group. Nominal composition: Si 0.7-1.3, Mg 0.6-1.2, Mn 0.4-1.0, Al rem. Typical uses: structural, machined parts (Europe/UK standard bar). Equivalents: AA 6082 (A96082) (USA), AlMgSi1 (3.2315) (Germany), H30 (UK).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/en-aw-6082
EN AW-6082 EN AW-AlSi1MgMn
EN 573-3 / EN 485 / EN 755
Chemical composition
EN AW-6082 — nominal composition
Weight %, to EN 573-3 / EN 485 / EN 755. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Si | 0.7-1.3 |
| Mg | 0.6-1.2 |
| Mn | 0.4-1.0 |
| Al | rem |
Mechanical & physical properties
EN AW-6082 — properties
Values shown are for 6082, the same alloy in another standard. Limits for EN AW-6082 may differ slightly — the standard on your drawing governs.
| Tensile strength, typical | 340 MPa |
| Yield / 0.2 % proof stress, typical | 310 MPa |
| Elongation, typical | 11 % |
| Brinell hardness, typical | 95 HB |
| Density at 20 °C | 2.7 g/cm³ |
| Melting range (solidus–liquidus) | 575–650 °C |
| Electrical conductivity at 20 °C | 40 % IACS |
| Thermal conductivity at 20 °C | 180 W/m·K |
Source: T6, Aluminum Association typical (typical values).
International equivalents
EN AW-6082 cross-reference
| System | Designation |
|---|---|
| Europe (this grade) | EN AW-6082 · EN AW-AlSi1MgMn |
| USA · UNS / ASTM | AA 6082 (A96082) |
| Germany · DIN | AlMgSi1 (3.2315) |
| UK · BS | H30 |
| Japan · JIS | — |
| China · GB | — |
⚠️ Relationship: Family match. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ Structural
- ▸ Machined parts (Europe/UK standard bar)
Product forms: Bar, extrusion, plate, sheet
EN AW-6082 parts
EN AW-6082 is a wrought grade (bar, rod, forging): we supply parts CNC machined from bar or forged — it is not used for castings. For a cast part, choose a cast grade.
More al-mg-si (6xxx) - structural & machining
Specification
How to specify EN AW-6082 on a drawing or order
- ▸ Grade and standard: EN 573-3 / EN 485 / EN 755 – EN AW-6082 / EN AW-AlSi1MgMn.
- ▸ Temper and size: state the temper (for example R360 / H080) when strength or hardness matters.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204
EN AW-6082 — questions buyers ask
What is EN AW-6082?+
EN AW-6082 (EN AW-AlSi1MgMn) is a wrought al-si-mg-mn 6082 alloy to EN 573-3 / EN 485 / EN 755, in the al-mg-si (6xxx) - structural & machining group. Nominal composition: Si 0.7-1.3, Mg 0.6-1.2, Mn 0.4-1.0, Al rem. Typical uses: structural, machined parts (Europe/UK standard bar). Equivalents: AA 6082 (A96082) (USA), AlMgSi1 (3.2315) (Germany), H30 (UK).
What are the equivalents of EN AW-6082?+
USA: AA 6082 (A96082); Germany: AlMgSi1 (3.2315); UK: H30. Relationship: Family match. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of EN AW-6082?+
Tensile strength, typical: 340 MPa; Yield / 0.2 % proof stress, typical: 310 MPa; Elongation, typical: 11 %; Brinell hardness, typical: 95 HB. Source: T6, Aluminum Association typical (typical values).
Does Conex supply parts in EN AW-6082?+
EN AW-6082 is a wrought grade (bar, rod, sheet or forging stock). We machine and supply finished parts in it to your drawing, and can recommend the matching cast grade if you need a casting instead.
How do I specify EN AW-6082 on a drawing?+
Write the standard and the grade together, for example "EN 573-3 / EN 485 / EN 755 – EN AW-6082 (EN AW-AlSi1MgMn)", and the temper. Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: EN 573-3 / EN 485 / EN 755 — Current.
- ▸ Properties: T6, Aluminum Association typical (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order EN AW-6082
Indicative $6/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.