Casting alloy · Germany · DIN 17445
G-X6CrNiMo18 10 G-X6CrNiMo18 10
G-X6CrNiMo18 10 (G-X6CrNiMo18 10) is a casting cast austenitic 316 (cf8m) alloy to DIN 17445 (legacy) - now DIN EN 10283, in the austenitic stainless castings (cf8 / cf3 / cf8m / cf3m) group. Nominal composition: C <= 0.08, Cr 18-21, Ni 9-12, Mo 2.0-3.0, Mn <= 1.5, Si <= 1.5. Equivalents: CF8M (USA), 1.4408 (Europe), 316C16 (UK), SCS14 (Japan).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/g-x6crnimo18-10
G-X6CrNiMo18 10 G-X6CrNiMo18 10
DIN 17445 (legacy) - now DIN EN 10283
Chemical composition
G-X6CrNiMo18 10 — nominal composition
Weight %, to DIN 17445 (legacy) - now DIN EN 10283. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| C | ≤ 0.08 |
| Cr | 18-21 |
| Ni | 9-12 |
| Mo | 2.0-3.0 |
| Mn | ≤ 1.5 |
| Si | ≤ 1.5 |
Mechanical & physical properties
G-X6CrNiMo18 10 — properties
Values shown are for CF8M, the same alloy in another standard. Limits for G-X6CrNiMo18 10 may differ slightly — the standard on your drawing governs.
| Tensile strength, min. | 485 MPa |
| Yield / 0.2 % proof stress, min. | 205 MPa |
| Elongation, min. | 30 % |
| Brinell hardness, typical | 140 HB |
| Density at 20 °C | 7.9 g/cm³ |
| Melting range (solidus–liquidus) | 1400–1450 °C |
| Thermal conductivity at 20 °C | 16.3 W/m·K |
Source: ASTM A351, solution annealed (minimum values).
International equivalents
G-X6CrNiMo18 10 cross-reference
| System | Designation |
|---|---|
| Germany (this grade) | G-X6CrNiMo18 10 · G-X6CrNiMo18 10 · also known as 1.4408 |
| USA · UNS / ASTM | CF8M |
| Europe · EN | 1.4408 |
| UK · BS | 316C16 |
| Japan · JIS | SCS14 |
| China · GB | ZG08Cr18Ni12Mo2 |
⚠️ Relationship: Family match. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs. This cross-reference should be verified against the controlling standard before certification.
Typical applications
- ▸ General engineering parts
Casting methods: Sand / investment / centrifugal
How we cast G-X6CrNiMo18 10
Every casting machined and inspected in-house.
Same alloy in other standards
Grades from the same cross-reference group.
More austenitic stainless castings (cf8 / cf3 / cf8m / cf3m)
Specification
How to specify G-X6CrNiMo18 10 on a drawing or order
- ▸ Grade and standard: DIN 17445 – G-X6CrNiMo18 10 / G-X6CrNiMo18 10.
- ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204 · ISO 8062-3
G-X6CrNiMo18 10 — questions buyers ask
What is G-X6CrNiMo18 10?+
G-X6CrNiMo18 10 (G-X6CrNiMo18 10) is a casting cast austenitic 316 (cf8m) alloy to DIN 17445 (legacy) - now DIN EN 10283, in the austenitic stainless castings (cf8 / cf3 / cf8m / cf3m) group. Nominal composition: C <= 0.08, Cr 18-21, Ni 9-12, Mo 2.0-3.0, Mn <= 1.5, Si <= 1.5. Equivalents: CF8M (USA), 1.4408 (Europe), 316C16 (UK), SCS14 (Japan).
What are the equivalents of G-X6CrNiMo18 10?+
USA: CF8M; Europe: 1.4408; UK: 316C16; Japan: SCS14; China: ZG08Cr18Ni12Mo2. Relationship: Family match. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of G-X6CrNiMo18 10?+
Tensile strength, min.: 485 MPa; Yield / 0.2 % proof stress, min.: 205 MPa; Elongation, min.: 30 %; Brinell hardness, typical: 140 HB. Source: ASTM A351, solution annealed (minimum values).
Can Conex cast G-X6CrNiMo18 10?+
Yes. We cast G-X6CrNiMo18 10 by sand casting, investment casting, centrifugal casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.
How do I specify G-X6CrNiMo18 10 on a drawing?+
Write the standard and the grade together, for example "DIN 17445 – G-X6CrNiMo18 10 (G-X6CrNiMo18 10)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: DIN 17445 (legacy) - now DIN EN 10283 — Legacy.
- ▸ Properties: ASTM A351, solution annealed (minimum values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order G-X6CrNiMo18 10
Indicative $8/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.