4 grades · 4 cast
Martensitic Stainless Castings (CA15 / 410 type)
Hardenable 13% chromium cast stainless for valve trim, pump and wear parts. 4 grades across USA, European, German, British, Japanese and Chinese standards — each with its own datasheet and cross-reference.
4 of 4 grades
| Grade | Name | System | Form | Composition |
|---|---|---|---|---|
| CA15● data | CA15 | USA · ACI cast grade | Cast | C <= 0.15, Cr 11.5-14, Ni <= 1.0, Mo <= 0.5 |
| 1.4011● data | GX12Cr12 | Europe · EN 10283:2019 stainless steel castings | Cast | C <= 0.15, Cr 11.5-14, Ni <= 1.0, Mo <= 0.5 |
| G-X12Cr14● data | G-X12Cr14 | Germany · DIN 17445 | Cast | C <= 0.15, Cr 11.5-14, Ni <= 1.0, Mo <= 0.5 |
| 410C21● data | 410C21 | UK · BS 3100 | Cast | C <= 0.15, Cr 11.5-14, Ni <= 1.0, Mo <= 0.5 |
Overview
Martensitic stainless steel castings are iron-chromium alloys with about 11.5–14% chromium and up to 0.15% carbon — typified by ASTM CA15, the cast counterpart of wrought 410 — that can be hardened and tempered by heat treatment to give much higher strength, hardness and wear and erosion resistance than austenitic stainless steels, with moderate corrosion resistance. They are used where strength and resistance to wear, erosion or cavitation matter more than maximum corrosion resistance: valve trim, pump impellers and wear rings, steam-turbine and hydro components, shafts, bushings and cutting or scraping parts.
The library lists CA15 with its German (1.4011, G-X12Cr14) and British (410C21) equivalents. This guide explains how martensitic stainless works, how heat treatment sets its properties, how CA15 compares with austenitic CF8M and with the tougher 13Cr-4Ni grade CA6NM, and what to specify when ordering.
The metallurgy in plain words
- Chromium (about 11.5–14%) — enough to make the steel stainless in mild environments by forming a passive oxide film, but less than austenitic grades, so corrosion resistance is lower.
- Carbon (up to 0.15%) — allows the steel to be hardened. When heated to a high temperature, the structure becomes austenite; on cooling it transforms to hard martensite, much like carbon steel.
- Nickel (up to about 1%) and molybdenum (up to about 0.5%) — small amounts improve toughness and hardenability.
- No significant nickel for austenite stability — so the steel is fully magnetic, unlike CF grades.
As-cast CA15 is hard but brittle and unstable. Its useful properties come only after a controlled hardening and tempering cycle.
Heat treatment: where the properties come from
- Austenitizing. The casting is heated to a high temperature (typically above about 950 °C) so the structure becomes austenite.
- Quenching. It is cooled in air or oil; CA15 hardens readily, so air cooling is often enough for moderate sections.
- Tempering. It is reheated to a lower temperature to trade some hardness for toughness and ductility. Higher tempering temperatures give lower hardness and higher toughness. Specifications such as ASTM A743 and A217 set minimum tempering temperatures for their classes.
Typical properties
ASTM A743 sets minimum properties for CA15 in the hardened-and-tempered condition. Values depend strongly on the tempering temperature; the governing standard and material test certificate apply.
| Property | CA15, hardened and tempered (A743 minimum) | CA15, tempered to higher hardness (typical range) | CF8M for comparison (A351 minimum) |
|---|---|---|---|
| Tensile strength | 620 MPa | Up to about 1,000+ MPa | 485 MPa |
| 0.2% proof strength | 450 MPa | Up to about 800+ MPa | 205 MPa |
| Elongation | 18% | Lower | 30% |
| Hardness | Typically about 200–260 HB | Up to about 40 HRC | About 150–170 HB |
| Magnetic | Yes | Yes | Slightly |
| Corrosion resistance | Moderate — atmosphere, fresh water, steam, mild chemicals | Good — including chlorides | |
CA15 compared with other stainless casting options
| Aspect | CA15 (13Cr martensitic) | CA6NM (13Cr-4Ni martensitic) | CF8M (austenitic) |
|---|---|---|---|
| Strength | High | High | Moderate |
| Hardness / wear | High | Moderate–high | Low |
| Toughness | Moderate | Very good | Excellent |
| Weldability | Difficult — preheat and post-weld heat treatment needed | Good with procedure | Very good |
| Corrosion resistance | Moderate | Moderate–good | Good |
| Cavitation / erosion | Good | Very good | Fair |
| Typical uses | Valve trim, wear rings, shafts, steam parts | Hydro-turbine runners, large pump impellers | Corrosion-resistant pump and valve bodies |
CA6NM is not in the current library list but can be supplied to specification; it is often the better choice for large, welded or impact-loaded parts.
Casting methods that suit martensitic stainless
- Investment casting — valve trim, small impellers, wear rings and precision parts.
- Resin sand and shell molding — larger impellers, casings and housings.
- Centrifugal casting — rings and sleeves.
Martensitic stainless is prone to cracking if cooled unevenly, so castings are usually cooled carefully and heat treated promptly. Conex casts stainless steel by investment and resin-sand/shell processes, heat treats to the specified condition, and machines in-house.
Applications by industry
| Industry | Parts |
|---|---|
| Valves | Trim — seats, discs, plugs, stems — for water, steam and oil service |
| Pumps | Impellers, wear rings, sleeves for abrasive or erosive water |
| Power generation | Steam-turbine parts, nozzles, diaphragm components |
| Oil & gas | Valve trim and components in mild environments |
| Food & process machinery | Scraper blades, cutting parts, wear components |
| General engineering | Shafts, bushings, levers needing strength plus rust resistance |
How to choose CA15
- Do you need more strength, hardness or erosion resistance than CF8M offers? If yes, consider CA15.
- Is the environment mild — atmosphere, steam, fresh water, oils? CA15 is suitable; for chlorides and acids, austenitic or duplex grades are safer.
- Will the part be welded or see impact? Consider CA6NM instead.
- Does the part slide against another stainless part? CA15's hardness reduces galling against austenitic mating parts.
Equivalents across standards
| ASTM | DIN (old) / EN number | BS 3100 (withdrawn) | JIS |
|---|---|---|---|
| CA15 (A743 / A217) | G-X12Cr14 / 1.4011 (as listed in the library; EN 10283 grades in the 1.40xx range are close) | 410C21 | SCS1 |
Equivalents are approximate; carbon, nickel and heat-treatment requirements differ. Quote the governing standard and class.
Design and machining tips
- Uniform sections reduce distortion and cracking during hardening.
- Machine before or after hardening? Rough machine before hardening and finish after, or machine fully in the tempered condition if hardness allows.
- Allow for distortion during heat treatment on long or thin parts.
- Use carbide tooling for hardened material; grinding may be needed for the hardest conditions.
- Surface finish matters: smooth, passivated surfaces resist rust better; rough or contaminated surfaces rust first.
- Welding requires preheat, controlled interpass temperature and post-weld heat treatment.
Common mistakes
- Expecting 316-level corrosion resistance from CA15.
- Ordering without a heat-treatment condition or hardness range.
- Welding without procedure, leading to cracking.
- Using CA15 for large impact-loaded parts where CA6NM would be tougher.
- Leaving machined surfaces unpassivated in humid environments.
Quality checks and documents
Each heat is analyzed by spectrometer; heat-treatment records are kept; hardness is tested on each lot and tensile tests are performed on test bars as required. Dimensional, visual and NDT inspections (dye-penetrant, magnetic particle — possible because CA15 is magnetic — and radiography) are arranged to specification. Material test certificates (EN 10204 3.1 on request) are supplied under an ISO 9001:2015 quality system.
Ordering checklist
- Drawing with critical dimensions and machined surfaces.
- Grade, standard and class (for example CA15 to ASTM A743 or A217).
- Heat-treatment condition and required hardness range.
- Service: medium, temperature, wear or erosion conditions.
- NDT, pressure test and certificate requirements; quantity.
Hardness, toughness and tempering choices
CA15 and related martensitic grades are useful because their properties can be tuned by heat treatment. After hardening, the steel is very hard but brittle; tempering restores toughness. Tempering at lower temperatures keeps high hardness for wear resistance, while tempering at higher temperatures gives better toughness and ductility for parts under impact. There is a temperature range where toughness and corrosion resistance can both suffer, so the tempering temperature should be chosen deliberately and stated on the drawing or agreed with the foundry. Buyers should specify the hardness range they need rather than leaving it open.
Corrosion behavior compared with austenitic grades
With around 12 to 14 percent chromium and little or no nickel, martensitic stainless steels resist atmospheric corrosion, fresh water, steam and mild chemicals, but they are clearly less resistant than CF8 or CF8M in chlorides, seawater and acids. They are chosen where strength, hardness and wear resistance matter more than maximum corrosion resistance: pump shafts and impellers in clean water, valve trim, steam turbine parts and cutting or wear components. Where both corrosion resistance and higher strength are needed, CA6NM, a lower-carbon grade with nickel and molybdenum, or duplex grades may be better choices.
Welding and repair
Martensitic stainless castings can be welded and repaired, but they need care. Preheating, controlled interpass temperatures and post-weld heat treatment are usually required to avoid cracking and to restore properties in the heat-affected zone. Weld repairs of castings should follow an approved procedure, and the drawing or purchase order should state whether repair welding is allowed and what inspection follows it.
Specifying CA15 on a drawing
A typical callout reads: "Stainless steel casting ASTM A743 grade CA15 (or A487 CA15M for pressure-containing parts), hardened and tempered to 200 to 250 HB". For European buyers, the equivalent is often GX12Cr12 (1.4011) to EN 10283. Add NDT requirements, heat treatment certification and the material test certificate type.
Working with Conex on martensitic stainless
Conex produces stainless steel castings by sand, shell and investment casting in Jamnagar, heat treats them to the specified condition and machines them in-house on CNC equipment. Each lot can be supplied with chemical analysis, hardness and mechanical test results, heat treatment records and a material test certificate to EN 10204 3.1, under an ISO 9001:2015 quality system, to customers in more than 34 countries.
Where CA15 is commonly used
Typical CA15 castings include pump impellers, casings and wear rings for clean water and condensate, valve bodies, discs and seats for steam and water service, turbine blades and nozzles, mixer blades and agitator parts that need wear resistance, food-machinery cutting parts where hardness matters, and general engineering parts that need more strength than austenitic stainless can provide. In each case the combination of moderate corrosion resistance and high hardness after heat treatment is the reason for choosing it.
Machining hardened castings
Martensitic castings are often rough machined in the annealed or soft condition, then hardened and tempered, and finally finish ground or machined. Machining directly in the hardened condition is possible with suitable tools but is slower. Planning the machining sequence with the heat treatment avoids distortion and saves cost. Drawings should state which surfaces are finished after heat treatment.
Testing CA15 castings
Typical checks include chemical analysis of each heat, hardness testing after heat treatment on every part or a sample per lot, tensile and impact tests on test bars when specified, dye penetrant or magnetic particle inspection of critical surfaces (martensitic stainless is magnetic, so magnetic particle testing is possible), and radiography for pressure-containing parts. Results are reported on the material test certificate, together with heat treatment details such as temperatures and times, so the buyer can confirm that the castings were processed as specified.
Ordering CA15 castings
Send the drawing with grade, required hardness range, heat treatment condition, machining stage, NDT and pressure test needs, and quantity. If the castings will be hardened after rough machining, mark which faces are finished later so the right allowances are left. For replacement parts, include the worn part or its old drawing and note where it failed.
Before you send an enquiry
A short list of facts helps choose the right grade from this family and quote accurately the first time:
- The part and its job: what it does, what it touches, and what a failure would cost in downtime or safety.
- Service conditions: fluid or environment, temperature range, pressure, loads, speed and lubrication.
- Grade or standard on the drawing: the UNS, EN, BS, JIS, GB, DIN or IS designation, or the old grade name if that is all you have.
- Process or stock form: sand, shell or investment casting. The most economical route can be suggested for your quantity.
- Machining stage: rough cast, semi-finished with allowance, or fully finished to drawing.
- Tests and documents: chemical analysis, mechanical and hardness tests, pressure test, NDT, material test certificate type (EN 10204 3.1), dimensional report and any third-party inspection.
- Quantities and timing: prototype, first batch, annual volume and delivery schedule.
- Market rules: any lead limit, drinking-water approval, RoHS or REACH requirement in the destination market.
With these details, the grade can be confirmed against the options covered on this page, or an equivalent suggested where it gives better value or performance for the same job.
Frequently asked questions
What is CA15 stainless steel?
CA15 is the ASTM designation for a cast 12–14% chromium martensitic stainless steel, the cast equivalent of wrought 410. It can be hardened and tempered.
Is CA15 magnetic?
Yes. Martensitic stainless steels are fully magnetic.
Is CA15 more corrosion resistant than CF8M?
No. CA15 has lower chromium and no molybdenum, so it is less corrosion resistant, but it is stronger and harder.
Can CA15 be welded?
Yes, but it needs a qualified procedure with preheat and post-weld heat treatment to avoid cracking and restore properties.
What is the difference between CA15 and CA6NM?
CA6NM contains about 4% nickel and less carbon, giving much better toughness and weldability. It is preferred for large hydro-turbine and pump parts; CA15 is harder and suits wear parts and valve trim.
What hardness can CA15 reach?
Depending on tempering, from roughly 200 HB in the tough condition up to around 40 HRC in harder conditions.
Why does CA15 rust in some environments?
With about 12–14% chromium and no molybdenum, its passive film is weaker than that of austenitic grades. Chlorides, stagnant water and rough or contaminated surfaces can cause rust spots.
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.