Casting alloy · China · GB/T 1176-2013
ZCuAl8Mn14Fe3Ni2 ZCuAl8Mn14Fe3Ni2
ZCuAl8Mn14Fe3Ni2 (ZCuAl8Mn14Fe3Ni2) is a casting aluminum bronze / nickel aluminum bronze alloy to GB/T 1176-2013 (cast copper and copper alloys), in the aluminum & nickel-aluminum bronze group. Nominal composition: Al 7.4–8.1, Mn 12.4–13.2, Fe 2.6–3.5, Ni 1.9–2.3, Cu rem. Typical uses: ship propellers.
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/zcual8mn14fe3ni2
ZCuAl8Mn14Fe3Ni2 ZCuAl8Mn14Fe3Ni2
GB/T 1176-2013 (cast copper and copper alloys)
Chemical composition
ZCuAl8Mn14Fe3Ni2 — nominal composition
Weight %, to GB/T 1176-2013 (cast copper and copper alloys). Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Al | 7.4–8.1 |
| Mn | 12.4–13.2 |
| Fe | 2.6–3.5 |
| Ni | 1.9–2.3 |
| Cu | rem |
Mechanical & physical properties
ZCuAl8Mn14Fe3Ni2 — properties
Values shown are for C95700, the same alloy in another standard. Limits for ZCuAl8Mn14Fe3Ni2 may differ slightly — the standard on your drawing governs.
| Tensile strength, min. | 620 MPa |
| Yield / 0.2 % proof stress, min. | 275 MPa |
| Elongation, min. | 20 % |
| Brinell hardness, typical | 180 HB |
| Density at 20 °C | 7.53 g/cm³ |
| Melting range (solidus–liquidus) | 954–988 °C |
| Electrical conductivity at 20 °C | 3 % IACS |
| Thermal conductivity at 20 °C | 12 W/m·K |
Source: ASTM B148 sand cast (minimum values).
International equivalents
ZCuAl8Mn14Fe3Ni2 cross-reference
| System | Designation |
|---|---|
| China (this grade) | ZCuAl8Mn14Fe3Ni2 · ZCuAl8Mn14Fe3Ni2 |
| USA · UNS / ASTM | — |
| Europe · EN | — |
| Germany · DIN | — |
| UK · BS | — |
| Japan · JIS | — |
⚠️ Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ Ship propellers
Casting methods: Sand, metal mold, centrifugal
How we cast ZCuAl8Mn14Fe3Ni2
Every casting machined and inspected in-house.
More aluminum & nickel-aluminum bronze
Specification
How to specify ZCuAl8Mn14Fe3Ni2 on a drawing or order
- ▸ Grade and standard: GB/T 1176-2013 – ZCuAl8Mn14Fe3Ni2 / ZCuAl8Mn14Fe3Ni2.
- ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204 · ISO 8062-3
ZCuAl8Mn14Fe3Ni2 — questions buyers ask
What is ZCuAl8Mn14Fe3Ni2?+
ZCuAl8Mn14Fe3Ni2 (ZCuAl8Mn14Fe3Ni2) is a casting aluminum bronze / nickel aluminum bronze alloy to GB/T 1176-2013 (cast copper and copper alloys), in the aluminum & nickel-aluminum bronze group. Nominal composition: Al 7.4–8.1, Mn 12.4–13.2, Fe 2.6–3.5, Ni 1.9–2.3, Cu rem. Typical uses: ship propellers.
What are the equivalents of ZCuAl8Mn14Fe3Ni2?+
ZCuAl8Mn14Fe3Ni2 has no published direct equivalent in the other systems we track. Send us your drawing and we will confirm the nearest grade.
What is the tensile strength of ZCuAl8Mn14Fe3Ni2?+
Tensile strength, min.: 620 MPa; Yield / 0.2 % proof stress, min.: 275 MPa; Elongation, min.: 20 %; Brinell hardness, typical: 180 HB. Source: ASTM B148 sand cast (minimum values).
Can Conex cast ZCuAl8Mn14Fe3Ni2?+
Yes. We cast ZCuAl8Mn14Fe3Ni2 by sand casting, centrifugal casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.
How do I specify ZCuAl8Mn14Fe3Ni2 on a drawing?+
Write the standard and the grade together, for example "GB/T 1176-2013 – ZCuAl8Mn14Fe3Ni2 (ZCuAl8Mn14Fe3Ni2)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: GB/T 1176-2013 (cast copper and copper alloys).
- ▸ Properties: ASTM B148 sand cast (minimum values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order ZCuAl8Mn14Fe3Ni2
Indicative $14/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.