Casting alloy · Europe · EN 1982:2017
CC494K CuSn5Pb9-C
CC494K (CuSn5Pb9-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the leaded bearing bronze group. Nominal composition: Sn 4–6, Pb 8–10, Zn ≤ 2, Cu rem. Typical uses: general bearings, bushes. Equivalents: C93500 (USA), LB4 (UK), CAC602 (nearest) (Japan), ZCuPb9Sn5 (China).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/cc494k
CC494K CuSn5Pb9-C
EN 1982:2017 (ingots CB…-B / castings CC…-C)
Chemical composition
CC494K — nominal composition
Weight %, to EN 1982:2017 (ingots CB…-B / castings CC…-C). Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Sn | 4–6 |
| Pb | 8–10 |
| Zn | ≤ 2 |
| Cu | rem |
Mechanical & physical properties
CC494K — properties
Values shown are for the nearest US grade C93500. EN limits for CC494K may differ slightly — the standard on your drawing governs.
| Tensile strength, min. | 207 MPa |
| Yield strength (0.5 % ext.), min. | 110 MPa |
| Elongation in 50 mm, min. | 12 % |
| Brinell hardness (500 kg), typical | 60 HB |
| Density at 20 °C | 8.86 g/cm³ |
| Melting range (solidus–liquidus) | 854–999 °C |
| Electrical conductivity at 20 °C | 15 % IACS |
| Thermal conductivity at 20 °C | 70.4 W/m·K |
| Thermal expansion (20–200 °C) | 17.1 ×10⁻⁶/K |
| Machinability rating | 70 (free-cutting brass C36000 = 100) |
Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
International equivalents
CC494K cross-reference
| System | Designation |
|---|---|
| Europe (this grade) | CC494K · CuSn5Pb9-C |
| USA · UNS / ASTM | C93500 |
| Germany · DIN | — |
| UK · BS | LB4 |
| Japan · JIS | CAC602 (nearest) |
| China · GB | ZCuPb9Sn5 |
⚠️ Relationship: Nearest. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ General bearings
- ▸ Bushes
Casting methods: GS, GM, GZ, GC (sand, permanent mold, centrifugal, continuous)
How we cast CC494K
Every casting machined and inspected in-house.
Same alloy in other standards
Grades from the same cross-reference group.
More leaded bearing bronze
In-depth guide
High-Leaded Tin Bronze C93500
Processes, parts, industries and prices for this alloy at Conex.
Read the Leaded Tin Bronze C93500 guide →Specification
How to specify CC494K on a drawing or order
- ▸ Grade and standard: EN 1982:2017 – CC494K / CuSn5Pb9-C.
- ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 1982 · EN 10204 · ISO 8062-3
CC494K — questions buyers ask
What is CC494K?+
CC494K (CuSn5Pb9-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the leaded bearing bronze group. Nominal composition: Sn 4–6, Pb 8–10, Zn ≤ 2, Cu rem. Typical uses: general bearings, bushes. Equivalents: C93500 (USA), LB4 (UK), CAC602 (nearest) (Japan), ZCuPb9Sn5 (China).
What are the equivalents of CC494K?+
USA: C93500; UK: LB4; Japan: CAC602 (nearest); China: ZCuPb9Sn5. Relationship: Nearest. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of CC494K?+
Tensile strength, min.: 207 MPa; Yield strength (0.5 % ext.), min.: 110 MPa; Elongation in 50 mm, min.: 12 %; Brinell hardness (500 kg), typical: 60 HB. Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
Can Conex cast CC494K?+
Yes. We cast CC494K by sand casting, gravity die casting, centrifugal casting, continuous casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.
How do I specify CC494K on a drawing?+
Write the standard and the grade together, for example "EN 1982:2017 – CC494K (CuSn5Pb9-C)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: EN 1982:2017 (ingots CB…-B / castings CC…-C).
- ▸ Properties: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order CC494K
Indicative $13/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.