Casting alloy · Europe · EN 1982:2017
CC495K CuSn10Pb10-C
CC495K (CuSn10Pb10-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the leaded bearing bronze group. Nominal composition: Sn 9–11, Pb 8–11, Cu rem. Typical uses: high-load bearings, rolling-mill bearings. Equivalents: C93700 (USA), G-CuPb10Sn (Germany), LB2 (UK), CAC603 (Japan).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/cc495k
CC495K CuSn10Pb10-C
EN 1982:2017 (ingots CB…-B / castings CC…-C)
Chemical composition
CC495K — nominal composition
Weight %, to EN 1982:2017 (ingots CB…-B / castings CC…-C). Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Sn | 9–11 |
| Pb | 8–11 |
| Cu | rem |
Mechanical & physical properties
CC495K — properties
Values shown are for the nearest US grade C93700. EN limits for CC495K may differ slightly — the standard on your drawing governs.
| Tensile strength, min. | 241 MPa |
| Yield strength (0.5 % ext.), min. | 138 MPa |
| Elongation in 50 mm, min. | 6 % |
| Brinell hardness (500 kg), typical | 60 HB |
| Density at 20 °C | 8.86 g/cm³ |
| Melting range (solidus–liquidus) | 762–929 °C |
| Electrical conductivity at 20 °C | 10 % IACS |
| Thermal conductivity at 20 °C | 46.9 W/m·K |
| Thermal expansion (20–200 °C) | 17.8 ×10⁻⁶/K |
| Modulus of elasticity | 76 GPa |
| Machinability rating | 80 (free-cutting brass C36000 = 100) |
Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
International equivalents
CC495K cross-reference
| System | Designation |
|---|---|
| Europe (this grade) | CC495K · CuSn10Pb10-C |
| USA · UNS / ASTM | C93700 |
| Germany · DIN | G-CuPb10Sn |
| UK · BS | LB2 |
| Japan · JIS | CAC603 |
| China · GB | ZCuPb10Sn10 |
⚠️ Relationship: Published comparison. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ High-load bearings
- ▸ Rolling-mill bearings
Casting methods: GS, GM, GZ, GC (sand, permanent mold, centrifugal, continuous)
How we cast CC495K
Every casting machined and inspected in-house.
Same alloy in other standards
Grades from the same cross-reference group.
More leaded bearing bronze
In-depth guide
High-Leaded Tin Bronze C93700 / LB2
Processes, parts, industries and prices for this alloy at Conex.
Read the Leaded Tin Bronze C93700 guide →Specification
How to specify CC495K on a drawing or order
- ▸ Grade and standard: EN 1982:2017 – CC495K / CuSn10Pb10-C.
- ▸ Casting method: state it when properties matter — sand, centrifugal and continuous castings have different minimum values.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 1982 · EN 10204 · ISO 8062-3
CC495K — questions buyers ask
What is CC495K?+
CC495K (CuSn10Pb10-C) is a casting leaded / bearing bronze alloy to EN 1982:2017 (ingots CB…-B / castings CC…-C), in the leaded bearing bronze group. Nominal composition: Sn 9–11, Pb 8–11, Cu rem. Typical uses: high-load bearings, rolling-mill bearings. Equivalents: C93700 (USA), G-CuPb10Sn (Germany), LB2 (UK), CAC603 (Japan).
What are the equivalents of CC495K?+
USA: C93700; Germany: G-CuPb10Sn; UK: LB2; Japan: CAC603; China: ZCuPb10Sn10. Relationship: Published comparison. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of CC495K?+
Tensile strength, min.: 241 MPa; Yield strength (0.5 % ext.), min.: 138 MPa; Elongation in 50 mm, min.: 6 %; Brinell hardness (500 kg), typical: 60 HB. Source: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
Can Conex cast CC495K?+
Yes. We cast CC495K by sand casting, gravity die casting, centrifugal casting, continuous casting at our foundry in Jamnagar, India, machine it on our CNC lines and supply a material test certificate with every lot. Send your drawing with quantity for a quotation.
How do I specify CC495K on a drawing?+
Write the standard and the grade together, for example "EN 1982:2017 – CC495K (CuSn10Pb10-C)", and the casting method if it matters (sand, centrifugal, continuous…). Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: EN 1982:2017 (ingots CB…-B / castings CC…-C).
- ▸ Properties: Mechanical: ASTM B505 (minimum values, separately cast test bars). Physical: Copper Development Association (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order CC495K
Indicative $13/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.