Wrought alloy (bar, rod, sheet, forging) · Germany · DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672
2.0855 CuNi2Si
2.0855 (CuNi2Si) is a wrought precipitation-hardening alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the high-copper alloys (beryllium / chromium / zirconium copper) group. Nominal composition: Cu rem, Ni 1.6-2.5, Si 0.4-0.8. Typical uses: connector pins, overhead-line fittings, bolts. Equivalents: C64700 (USA), CW111C CuNi2Si (Europe).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/din-2-0855
2.0855 CuNi2Si
DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN
Chemical composition
2.0855 — nominal composition
Weight %, to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Cu | rem |
| Ni | 1.6-2.5 |
| Si | 0.4-0.8 |
Mechanical & physical properties
2.0855 — properties
Values shown are for C64700, the same alloy in another standard. Limits for 2.0855 may differ slightly — the standard on your drawing governs.
| Tensile strength, typical | 620 MPa |
| Yield / 0.2 % proof stress, typical | 550 MPa |
| Elongation, typical | 10 % |
| Brinell hardness, typical | 180 HB |
| Density at 20 °C | 8.86 g/cm³ |
| Melting range (solidus–liquidus) | 1040–1090 °C |
| Electrical conductivity at 20 °C | 40 % IACS |
| Thermal conductivity at 20 °C | 210 W/m·K |
Source: solution treated and aged, CDA / ASM handbook (typical values).
International equivalents
2.0855 cross-reference
| System | Designation |
|---|---|
| Germany (this grade) | 2.0855 · CuNi2Si |
| USA · UNS / ASTM | C64700 |
| Europe · EN | CW111C CuNi2Si |
| UK · BS | — |
| Japan · JIS | — |
| China · GB | — |
⚠️ Relationship: Nearest. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ Connector pins
- ▸ Overhead-line fittings
- ▸ Bolts
Product forms: Rod, bar, wire, sheet, strip, tube
2.0855 parts
2.0855 is a wrought grade (bar, rod, forging): we supply parts CNC machined from bar or forged — it is not used for castings. For a cast part, choose a cast grade.
More high-copper alloys (beryllium / chromium / zirconium copper)
Specification
How to specify 2.0855 on a drawing or order
- ▸ Grade and standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0855 / CuNi2Si.
- ▸ Temper and size: state the temper (for example R360 / H080) when strength or hardness matters.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204
2.0855 — questions buyers ask
What is 2.0855?+
2.0855 (CuNi2Si) is a wrought precipitation-hardening alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the high-copper alloys (beryllium / chromium / zirconium copper) group. Nominal composition: Cu rem, Ni 1.6-2.5, Si 0.4-0.8. Typical uses: connector pins, overhead-line fittings, bolts. Equivalents: C64700 (USA), CW111C CuNi2Si (Europe).
What are the equivalents of 2.0855?+
USA: C64700; Europe: CW111C CuNi2Si. Relationship: Nearest. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of 2.0855?+
Tensile strength, typical: 620 MPa; Yield / 0.2 % proof stress, typical: 550 MPa; Elongation, typical: 10 %; Brinell hardness, typical: 180 HB. Source: solution treated and aged, CDA / ASM handbook (typical values).
Does Conex supply parts in 2.0855?+
2.0855 is a wrought grade (bar, rod, sheet or forging stock). We machine and supply finished parts in it to your drawing, and can recommend the matching cast grade if you need a casting instead.
How do I specify 2.0855 on a drawing?+
Write the standard and the grade together, for example "DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0855 (CuNi2Si)", and the temper. Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN — Legacy DIN designation (W.Nr still widely quoted).
- ▸ Properties: solution treated and aged, CDA / ASM handbook (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order 2.0855
Indicative $19/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.